Hi All,

the hot water and heavy weight worked on this DCLi one. Pictures before and after..did the water and weight twice then sat for a while working the badge in fingers slowly pressing flat, heat from hands seemed just enough to warm the plastic for final manipulation. Good as it's going to get,but happy with it.

Many thanks for all suggestions,

Mark